* Update quality_settings_wall_generator.md * Expand layer height wiki * Rework height * Update quality_settings_line_width.md * Update quality_settings_precision.md * Update quality_settings_seam.md * Minor linking * Update quality_settings_wall_and_surfaces.md * Reverse on odd improved * Extra perimeter on overhangs * Images fixes * Update speed_settings_jerk_xy.md * quality_settings_ironing * Update quality_settings_seam.md * Update quality_settings_bridging.md * Remove precision sub-section links * Add icons to settings links in Home documentation * Moved fuzzy skin Remove Fuzzy Skin section from special mode settings to it's own place. * Fix image adaptive-pressure-advance-calib.md * Update image references Standardized image alt text and filenames for consistency and clarity. * Update image alt text and file references in docs Standardized and clarified image alt text in Calibration.md for easy md to html conversion. * Update seam * Base scarf joint seam * Update quality_settings_seam.md * Update quality_settings_wall_generator.md * Update quality_settings_overhangs.md * Fuzzy Skin Generator Mode Wiki Co-Authored-By: π² <189209038+pi-squared-studio@users.noreply.github.com> * Infill Templates Wiki Co-Authored-By: π² <189209038+pi-squared-studio@users.noreply.github.com> * basic md formating * Update infill and advanced strength settings docs * Moved + Linked Metalanguage * image preview (change befor ready) * Update strength_settings_infill_rotation_template_metalanguage.md * reorder image description * Some credits * Spelling infill rotation metalanguage docs * Crop metalanguage fills * fix image reference * Update strength_settings_infill_rotation_template_metalanguage.md * Update strength_settings_infill_rotation_template_metalanguage.md * standard characters images * flow rate update division * Update Tab.cpp * Reworking flow rate calibration guide * Update strength_settings_top_bottom_shells.md * Flow Calib WIP --------- Co-authored-by: π² <189209038+pi-squared-studio@users.noreply.github.com> Co-authored-by: pi-squared-studio <pi.squared.studio@gmail.com>
2.4 KiB
Layer Height
Layer height defines the vertical thickness of each printed layer, playing a crucial role in both print quality and printing speed.
Using smaller layer heights increases print time but results in:
- Smoother surface finishes
- Less noticeable layer lines
- Enhanced detail on curves
- Better performance on overhangs
Quick Reference
| Nozzle Size | Min | Max | First Layer Height |
|---|---|---|---|
| 0.2mm | 0.04mm | 0.16mm | 0.12mm |
| 0.3mm | 0.06mm | 0.24mm | 0.18mm |
| 0.4mm | 0.08mm | 0.32mm | 0.25mm |
| 0.5mm | 0.10mm | 0.40mm | 0.30mm |
| 0.6mm | 0.12mm | 0.48mm | 0.35mm |
| 0.8mm | 0.16mm | 0.64mm | 0.45mm |
| 1.0mm | 0.20mm | 0.80mm | 0.55mm |
Layer Height Guidelines
Usually, the optimal range for layer height is between 20% and 80% of the nozzle diameter.
- Below 20%: Flow inconsistencies and "fish scale" patterns may occur, especially at high speeds.
- Over 80%: Increased risk of layer adhesion issues and reduced print quality.
First Layer Height
Controls the thickness of the initial layer.
A thicker first layer improves bed adhesion and compensates for build surface imperfections.
Recommended: 0.25mm for 0.4mm nozzle (62.5% of nozzle diameter)
Maximum: 65% of nozzle diameter
Layer Height Overhangs Impacts
Layer height directly affects overhang angle capability and quality.
Smaller layer heights enable steeper overhangs by reducing the unsupported distance between layers, while larger layer heights increase this gap, leading to more sagging and requiring support material at shallower angles.