Cura/resources/quality/ultimaker3/um3_aa0.4_CPE_Draft_Print.inst.cfg
Ghostkeeper 050f76e11d
Update quality profiles from material research
This locks initial layer speed at 20, without scaling from the normal print speed. It also adjusts some jerk and speed of support infill.
2017-02-10 18:09:34 +01:00

25 lines
661 B
INI

[general]
version = 2
name = Draft Print
definition = ultimaker3
[metadata]
type = quality
quality_type = draft
material = generic_cpe_ultimaker3_AA_0.4
weight = -2
[values]
material_print_temperature = =default_material_print_temperature + 10
material_initial_print_temperature = =material_print_temperature - 5
material_final_print_temperature = =material_print_temperature - 10
material_standby_temperature = 100
prime_tower_size = 17
skin_overlap = 20
speed_print = 60
speed_layer_0 = 20
speed_topbottom = =math.ceil(speed_print * 35 / 60)
speed_wall = =math.ceil(speed_print * 45 / 60)
speed_wall_0 = =math.ceil(speed_wall * 35 / 45)
wall_thickness = 1