Paul agreed, this should not be dependent on the quality. It was meant to allow a bit slower prints due to the time it takes to do a retraction, but that is not the bottleneck here. Material hardness is the bottleneck. Grinding is. Contributes to issue CURA-346.
21 lines
404 B
Text
21 lines
404 B
Text
[general]
|
|
version = 1
|
|
name = Ulti Quality
|
|
machine_type = ultimaker2plus
|
|
machine_variant = 0.4 mm
|
|
material = PLA
|
|
weight = -4
|
|
|
|
[settings]
|
|
line_width = 0.35
|
|
layer_height = 0.04
|
|
layer_height_0 = 0.26
|
|
wall_thickness = 1.4
|
|
top_bottom_thickness = 1.12
|
|
infill_sparse_density = 25
|
|
speed_print = 30
|
|
speed_infill = 50
|
|
speed_wall_x = 40
|
|
speed_topbottom = 20
|
|
speed_layer_0 = 25
|
|
cool_min_layer_time_fan_speed_max = 15
|