[general]
version = 4
name = Fast
definition = ultimaker3
[metadata]
setting_version = 20
type = quality
quality_type = draft
weight = -2
material = generic_pp
variant = AA 0.8
[values]
brim_width = 25
cool_min_layer_time_fan_speed_max = 6
cool_min_speed = 17
top_skin_expand_distance = =line_width * 2
infill_pattern = ='zigzag' if infill_sparse_density > 80 else 'tetrahedral'
material_bed_temperature_layer_0 = =material_bed_temperature
material_print_temperature = =default_material_print_temperature - 2
multiple_mesh_overlap = 0.2
prime_tower_enable = True
prime_tower_flow = 100
prime_tower_min_volume = 10
retraction_count_max = 15
retraction_extra_prime_amount = 0.5
retraction_hop = 0.5
retraction_min_travel = 1.5
retraction_prime_speed = 15
speed_travel = 300
speed_wall_x = =math.ceil(speed_wall * 30 / 30)
switch_extruder_prime_speed = 15
switch_extruder_retraction_amount = 20
switch_extruder_retraction_speeds = 45
top_bottom_thickness = 1.6
wall_0_wipe_dist = =line_width * 2