[general] version = 1 name = Fast Prints machine_type = Ultimaker 2+ machine_variant = 0.4mm Nozzle material = CPE [settings] cool_fan_speed_min = 50 retraction_hop = 0.0 skin_no_small_gaps_heuristic = False raft_airgap = 0.0 speed_travel = 150 raft_surface_thickness = 0.27 raft_interface_line_spacing = 3.0 support_enable = False raft_surface_line_width = 0.4 raft_surface_line_spacing = 3.0 retraction_combing = All adhesion_type = brim cool_min_layer_time = 3 layer_height = 0.15 raft_margin = 5.0 speed_infill = 45 bottom_thickness = 0.75 brim_line_count = 20 cool_lift_head = True retraction_speed = 40.0 cool_fan_speed_max = 100 magic_mesh_surface_mode = False speed_print = 30 shell_thickness = 0.7 speed_wall_0 = 30 material_flow = 100.0 support_pattern = lines infill_sparse_density = 18 raft_interface_line_width = 0.4 layer_height_0 = 0.26 material_bed_temperature = 70 top_thickness = 0.75 top_bottom_thickness = 0.75 speed_wall_x = 40 infill_overlap = 17 infill_before_walls = False skirt_minimal_length = 150.0 speed_topbottom = 20 skirt_gap = 3.0 raft_base_line_width = 1.0 machine_nozzle_size = 0.35