PLA 0.8mm Faster printing

Optimization for faster printing with the 0.8mm profiles for PLA. Also removed retract at layer change for less artifacts, and changed infill pattern to triangular for more unity between profiles.
This commit is contained in:
THeijmans 2018-02-07 16:09:57 +01:00
parent 014c2628bb
commit 97c96ab2da
3 changed files with 12 additions and 6 deletions

View file

@ -15,8 +15,8 @@ cool_fan_full_at_height = =layer_height_0 + 2 * layer_height
cool_fan_speed_max = =100
cool_min_speed = 2
gradual_infill_step_height = =3 * layer_height
infill_line_width = =round(line_width * 0.535 / 0.75, 2)
infill_pattern = cubic
infill_line_width = =round(line_width * 0.65 / 0.75, 2)
infill_pattern = triangles
line_width = =machine_nozzle_size * 0.9375
machine_nozzle_cool_down_speed = 0.75
machine_nozzle_heat_up_speed = 1.6
@ -25,6 +25,8 @@ material_initial_print_temperature = =max(-273.15, material_print_temperature -
material_print_temperature = =default_material_print_temperature + 10
material_standby_temperature = 100
prime_tower_enable = True
retract_at_layer_change = False
speed_print = 45
support_angle = 70
support_line_width = =line_width * 0.75
support_pattern = ='triangles'

View file

@ -15,8 +15,8 @@ cool_fan_full_at_height = =layer_height_0 + 2 * layer_height
cool_fan_speed_max = =100
cool_min_speed = 2
gradual_infill_step_height = =3 * layer_height
infill_line_width = =round(line_width * 0.535 / 0.75, 2)
infill_pattern = cubic
infill_line_width = =round(line_width * 0.65 / 0.75, 2)
infill_pattern = triangles
layer_height = 0.4
line_width = =machine_nozzle_size * 0.9375
machine_nozzle_cool_down_speed = 0.75
@ -27,6 +27,8 @@ material_print_temperature = =default_material_print_temperature + 15
material_standby_temperature = 100
prime_tower_enable = True
raft_margin = 10
retract_at_layer_change = False
speed_print = 45
support_angle = 70
support_line_width = =line_width * 0.75
support_pattern = ='triangles'

View file

@ -15,8 +15,8 @@ cool_fan_full_at_height = =layer_height_0 + 2 * layer_height
cool_fan_speed_max = =100
cool_min_speed = 2
gradual_infill_step_height = =3 * layer_height
infill_line_width = =round(line_width * 0.535 / 0.75, 2)
infill_pattern = cubic
infill_line_width = =round(line_width * 0.65 / 0.75, 2)
infill_pattern = triangles
layer_height = 0.3
line_width = =machine_nozzle_size * 0.9375
machine_nozzle_cool_down_speed = 0.75
@ -26,6 +26,8 @@ material_initial_print_temperature = =max(-273.15, material_print_temperature -
material_print_temperature = =default_material_print_temperature + 10
material_standby_temperature = 100
prime_tower_enable = True
retract_at_layer_change = False
speed_print = 45
support_angle = 70
support_line_width = =line_width * 0.75
support_pattern = ='triangles'