@ -16,12 +16,14 @@ material_print_temperature = =default_material_print_temperature + 10
material_initial_print_temperature = =material_print_temperature - 5
material_final_print_temperature = =material_print_temperature - 10
retraction_combing_max_distance = 50
skin_edge_support_thickness = =0.8 if infill_sparse_density < 30 else 0
skin_overlap = 20
speed_print = 60
speed_layer_0 = =math.ceil(speed_print * 20 / 60)
speed_topbottom = =math.ceil(speed_print * 35 / 60)
speed_wall = =math.ceil(speed_print * 45 / 60)
speed_wall_0 = =math.ceil(speed_wall * 35 / 45)
top_thickness = =0.8 if infill_sparse_density < 30 and skin_edge_support_thickness == 0.8 else top_bottom_thickness
wall_thickness = 1

View file

@ -19,6 +19,7 @@ machine_nozzle_heat_up_speed = 1.6
material_print_temperature = =default_material_print_temperature + 5
material_standby_temperature = 100
prime_tower_enable = False
skin_edge_support_thickness = =0.8 if infill_sparse_density > 30 else 0
skin_overlap = 20
speed_layer_0 = =math.ceil(speed_print * 20 / 70)
speed_topbottom = =math.ceil(speed_print * 40 / 70)